Stainless steel, duplex & superduplex
We offer an extensive range of special stainless steels, duplex and super duplex, particularly with material numbers 1.4462, 1.4410, 1.4501, 1.4313, 1.4418, 1.4835, 1.4539, 1.4547, 1.4003. Our strength: customised solutions! Thanks to our excellent business contacts, we can also supply large quantities on short notice.
Products
M.-nr. / EN | DIN | AISI | UNS | BS | AFNOR | GOST | |
---|---|---|---|---|---|---|---|
1.4000 | X6Cr13 | 410S | S41008 | 403 S 17 | X6Cr13 | 08X13 | |
ProductsStrips / foils
Sheets / plates
Round blanks / rings
Drawing profiles
Forgings
CompositionScopesoil industry
hydraulic turbines
Featureshighly resistant against hydrogen and sulphur
highly weldable with TIG and arc welding
filler metals 1.4009 + 1.4302, etc.
not resistant against intergranular corrosion
high resistance against corrosion in mirror polished or grinded condition
|
|||||||
1.4003 | X2Cr11 | 3Cr12 | S40977 | X2CrNi12 | X2CrNi12 | ||
ProductsSheets / plates
Pipes
Pipe fittings
Round blanks / rings
Forgings
Drawing profiles
Cuts (waterjet, plasma, shear, laser-cut or sawn)
CompositionC
≤ 0,03 %
Cr
min. 10,5 % / max. 12,5 %
Ni
min. 0,30 % / max. 1,0 %
Scopesconstruction industry
engineering
oil industry
automotive industry
mining industry
electronic equipment
transport industry
sugar industry
Featuresgood machinability
suited for use in mildly corrosive media
higher strengths than other ferrites, can be welded in thicker areas
cold heading grades
use at low temperatures
resistant to wet abrasion
limited use in temp. below 350°C
weldable, except oxyacetylene welding
filler metals: 1.4316 or 1.4370
|
|||||||
1.4006 | X12Cr13 | 410 | 410S21 | Z10C13 / Z13C13 | 12X13 | ||
ProductsStrips / foils
Sheets / plates
Round blanks / rings
Forgings
Bars
Drawing profiles
Cuts (waterjet, plasma, shear, laser-cut or sawn)
CompositionCr
min. 0,08 % / max. 0,15 %
Cr
min. 11,50 % / max. 13,50 %
Scopesoil industry
petrochemical industry
decorative and kitchen equipment
pump industry
hydraulic engineering
Featuresferromagnetic grade
good corrosion resistance in moderately aggressive media (soap, solvents and organic acids)
low susceptibility against embrittlement
good resistance in oxidizing atmospheres up to 600°C
available in annealed and tempered state
before welding. normally preheat to 100-300°C and temper after welding
|
|||||||
1.4034 | X46Cr13 | 420 | S42000 | 420S45 | Z44C14 / Z38C13 | 46X13 | |
ProductsStrips / foils
Sheets / plates
Round blanks / rings
Forgings
Bars
Drawing profiles
Cuts (waterjet, plasma, shear, laser-cut or sawn)
CompositionC
min. 0,43 % / max. 0,50 %
S
≤ 0,03 %
Cr
min. 12,50 % / max. 14,50 %
Scopesengineering
medical and pharmaceutical industry
cutlery industry
rolling bearing industry
Featuresgood corrosion resistance against water and water vapour
not resistant against intergranular corrosion in delivered state
best corrosion resistance in tempered state with polished surface
in general, do not weld 1.4034
good corrosion- resistance in moderately aggressive media (soap, solvents and organic acids)
|
|||||||
1.4112 | X90CrMoV18 | 440B | |||||
ProductsStrips / foils
Sheets / plates
Round blanks / rings
Forgings
Bars
Drawing profiles
Cuts (waterjet, plasma, shear, laser-cut or sawn)
CompositionC
≤ 0,90 %
Cr
≤ 18,0 %
Mo
≤ 1,10 %
V
≤ 0,10
Scopescutlery industry
perforated discs
screw elements
bearings
spray nozzle
hardened valves
Featureshigh tempering ability
wear-resistant
polishable
extremely high edge retention
|
|||||||
1.4122 | X39CrMo17-1 | ||||||
ProductsStrips / foils
Sheets / plates
Round blanks / rings
Forgings
Bars
Drawing profiles
Cuts (waterjet, plasma, shear, laser-cut or sawn)
CompositionC
min. 0,33 % / max. 0,45 %
Cr
min. 15,5 % / max. 17,5 %
Mo
min. 0,80 % / max. 1,30 %
Ni
≤ 1,00 %
Scopesconstruction industry
engineering
automotive industry
cutlery industry
food industry
pump shafts
Featuresferromagnetic grade
high gloss polishable
good corrosion resistance in mildly aggressive media and low chlorine ion concentration
without cathodic protection not seawater resistant
better corrosion resistance with polished or finely grinded surfaces
mechanical properties can be improved through annealing
usually not weldable
|
|||||||
1.4313 | X3CrNiMo13-4 | F6NM430 | J91540 | 425 C 11 | Z 6 CN 13-04 | 03X13H4M | |
ProductsSheets / plates
Round blanks / rings
Forgings
Bars
Cuts (waterjet, plasma, shear, laser-cut or sawn)
Drawing profiles
CompositionC
≤ 0,05 %
Cr
min. 12,0 % / max. 14,0 %
Mo
min. 0,30 % / max. 0,70 %
Ni
min. 3,5 % / max. 4,5 %
N
min. 0,02 %
Scopesoil industry
petrochemical industry
pump and compressor elements
turbines for water works
tools for casting
Featuresferromagnetic grade
superb mechanical properties
preheat work piece for welding to about 150°C
good corrosion resistance in moderate corrosion environments with no chlorides
much better corrosion resistance with polished surface
optimum processing properties after solution heat treatment at 600-650°C followed by slow cool down
slowly heat work piece for forging to 850°C, then more quickly to 1100-1150°C. Forging at 900-1150°C
machining depends on hardness and strength
|
|||||||
1.4362 | X2CrNiN23-4 | S32304 | Z 2 CN 23-04AZ | ||||
ProductsStrips / foils
Sheets / plates
Pipes
Round blanks / rings
Forgings
Drawing profiles
Cuts (waterjet, plasma, shear, laser-cut or sawn)
CompositionC
≤ 0,03 %
Cr
min. 22,0 % / max. 24,0 %
Mo
min. 0,10 % / max. 0,60 %
Ni
min. 3,5 % / max. 5,5 %
N
min. 0,05 % / max. 0,20 %
Cu
min. 0,10 % / max. 0,60 %
Scopesconstruction industry
oil industry
chemical + petrochemical industry
shipbuilding and engineering
Featuresweldable
duplex, magnetisable
to be used at -50-300°C
not sensitive to intergranular corrosion
superb resistance against stress corrosion
not polishable
only conditionally machinable
|
|||||||
1.4410 | X2CrNiMoN25-7-4 | F53 | S32750 | X2CrNiMoN25-7-4 | Z 3 CND 25.07Az | X2CrNiMoN25-7-4 | |
ProductsStrips / foils
Sheets / plates
Hollow steel
Pipes
Pipe fittings
Round blanks / rings
Forgings
Bars
Cuts (waterjet, plasma, shear, laser-cut or sawn)
Drawing profiles
CompositionC
≤ 0,03 %
Si
≤ 0,80 %
Mn
≤ 1,20 %
P
≤ 0,035 %
S
≤ 0,015 %
Cr
min. 24,0 % / max. 26,0 %
Mo
min. 3,0 % / max. 4,5 %
Ni
min. 6,0 % / max. 8,0 %
N
min. 0,24 % / max. 0,35 %
Cu
≤ 0,50 %
Scopesoffshore
desalination plants
piping construction
chemical + petrochemical industry
apparatus and container engineering
chemical tanks
Featuresduplex, magnetisable
superb resistance in contact with chloride-containing media
weldable (except gas welding)
excellent corrosion resistance
|
|||||||
1.4418 | X4CrNiMo16-5-1 | S165M | X4CrNiMo16-5-1 | Z 6 CND 16-05-01 | |||
ProductsSheets / plates
Round blanks / rings
Forgings
Bars
Cuts (waterjet, plasma, shear, laser-cut or sawn)
Drawing profiles
CompositionC
≤ 0,06 %
Cr
min. 15,0 % / max. 17,0 %
Mo
min. 0,80 % / max. 1,50 %
Ni
min. 4,0 % / max. 6,0 %
N
min. 0,02 %
Scopesengineering
chemical industry
shipbuilding
automotive industry (exhaust system)
aerospace industry
Featuressuperb corrosion resistance in aggressive media
magnetisable
limited use in maritime areas acceptable
extremely resistant against intergranular corrosion
highly resistant against fatigue and stress corrosion
weldable, however work piece preheating to about 100-200°C necessary
suitable for low temperatures
suitable up to 400°C
|
|||||||
1.4438 | X2CrNiMo18-15-4 | 317L | S31703 | 317 S 12 | X2CrNiMo18-15-4 | ||
ProductsStrips / foils
Sheets / plates
Profiles
Bars
Drawing profiles
CompositionC
≤ 0,03 %
Si
≤ 1,00 %
Mn
≤ 2,00 %
P
≤ 0,045 %
S
≤ 0,015 %
Cr
min. 17,5 % / max. 19,5 %
Mo
min. 3,00 % / max. 4,00 %
Ni
min. 13,0 % / max. 16,0 %
N
≤ 0,11 %
PaperScopeschemical industry
pulp industry
transport container for chemicals
Featureshigher corrosion resistance than AISI 316L, especially in highly corrosive environments with chlorides and halides
filler metals: 1.4440, 1.4438
|
|||||||
1.4462 | X2CrNiMoN22-5-3 | 318LN. F51 | S31803 | 318 S 13 | Z 2 CND 22-05Az | 03X22H5AM3 | |
ProductsStrips / foils
Sheets / plates
Hollow steel
Profiles
Pipes
Pipe fittings
Round blanks / rings
Forgings
Bars
Drawing profiles
Cuts (waterjet, plasma, shear, laser-cut or sawn)
Drawing profiles
CompositionC
≤ 0,03 %
Si
≤ 1,00 %
Mn
≤ 2,00 %
P
≤ 0,035 %
S
≤ 0,015 %
Cr
min. 21,0 % / max. 23,0 %
Mo
min. 2,5 % / max. 3,5 %
Ni
min. 4,5 % / max. 6,5 %
N
min. 0,1 % / max. 0,22 %
Scopesfood industry
offshore
desalination plants
paper and pulp industry
chemical and petrochemical industry
desalination plant
nuclear engineering
Featuresrust-free austenite, duplex with molybdenum additive, good resistance against pitting and intergranular corrosion
filler metal: 1.4462
temperature range 10-280 °C
hardness / HB30: ≤ 270
|
|||||||
1.4501 | F55 | S32760 | X2CrNiMoCuWN25-7-4 | Z 3 CND 25.06Az | X2CrNiMoCuWN25-7-4 | ||
ProductsStrips / foils
Sheets / plates
Pipes
Pipe fittings
Round blanks / rings
Forgings
Bars
Cuts (waterjet, plasma, shear, laser-cut or sawn)
Drawing profiles
CompositionC
≤ 0,03 %
Si
≤ 1,00 %
Mn
≤ 1,00 %
P
≤ 0,035 %
S
≤ 0,015 %
Cr
min. 24,0 % / max. 26,0 %
Mo
min. 3,0 % / max. 4,0 %
Ni
min. 6,0 % / max. 8,0 %
N
min. 0,20 % / max. 0,30 %
Cu
min. 0,50 % / max. 1,00 %
W
min. 0,50 % / max. 1,00 %
Fe
Bal.
Scopeschemical industry
petrochemistry
offshore
desalination plants
container construction
piping construction
chemical tanker construction
Featuresduplex
superb corrosion resistance in chloride containing media
weldable (except gas welding)
machining properties comparable with material 1.4462
polishable, but modified appearance of the polishing result is to be expected due to the two-phase structure
good resistance against surface-wide corrosion
comparable to common austenite grades, improved resistance against pitting and crevice corrosion
|
|||||||
1.4539 | X1NiCrMoCu25-20-5 | 904L | N08904 | 904 S 13 | Z2NCDU25-20 | ||
ProductsStrips / foils
Sheets / plates
Hollow steel
Pipes
Pipe fittings
Round blanks / rings
Forgings
Bars
Cuts (waterjet, plasma, shear, laser-cut or sawn)
Drawing profiles
CompositionC
≤ 0,02 %
Si
≤ 0,70 %
Mn
≤ 2,0 %
P
≤ 0,03 %
S
≤ 0,01 %
Cr
min. 19,0 % / max. 21,0 %
Mo
min. 4,0 % / max. 5,0 %
Ni
min. 24,0 % / max. 26,0 %
N
≤ 0,15 %
Cu
min. 1,20 % / max. 2,0 %
Scopeschemical industry
refinery
offshore
paper and pulp industry
seawater technology
Featuresexcellent resistance against intergranular corrosion, stress corrosion and pitting
filler metals: 1.4539, 1.4519
|
|||||||
1.4547 | X1CrNiMoCuN20-18-7 | 254SMO | S31254 | X1CrNiMoCuN20-18-7 | X1CrNiMoCuN20-18-7 | ||
ProductsStrips / foils
Sheets / plates
Pipes
Round blanks / rings
Forgings
Bars
Cuts (waterjet, plasma, shear, laser-cut or sawn)
Drawing profiles
CompositionC
≤ 0,02 %
Si
≤ 0,70 %
Mn
≤ 1,00 %
P
≤ 0,03 %
S
≤ 0,01 %
Cr
min. 19,5 % / max. 20,5 %
Mo
min. 6,0 % / max. 7,0 %
Ni
min. 17,5 % / max. 18,5 %
N
min. 0,18 % / max. 0,25 %
Cu
min. 0,50 % / max. 1,0 %
Fe
Rest
Scopesshipbuilding
offshore
desalination plants
paper and pulp industry
water treatment plants
Featuresweldable
machinable in annealed condition
tends towards strain hardening
excellent resistance against pitting, crevice corrosion and surface erosion
cannot be magnetized in solution annealed condition
cannot be cured by heat treatment
seawater resistant
|
|||||||
1.4550 | X6CrNiNb18-10 | 347, 347H | S34700 | 347 S 20 | X6CrNiNb18-10 | 08Ch18N12B | |
ProductsStrips / foils
Sheets / plates
Pipes
Pipe fittings
Round blanks / rings
Forgings
Bars
Drawing profiles
Cuts (waterjet, plasma, shear, laser-cut or sawn)
CompositionC
≤ 0,08 %
Si
≤ 1,00 %
Mn
≤ 2,00 %
P
≤ 0,045 %
S
≤ 0,015 %
Cr
min. 17,0 % / max. 19,0 %
Nb
10 x C
Ni
min. 9,00 % / max. 12,0 %
Scopesfood industry
chemical industry
Featuresgood resistance against intergranular corrosion
filler metals: 1.4316, 1.4551, 1.4576
|
|||||||
1.4713 | X10CrAl7 | Sicromal 8 | X10CrAlSi7 | 12X7CIO | |||
ProductsStrips / foils
Sheets / plates
Pipes
Round blanks / rings
Bars
Drawing profiles
Cuts (waterjet, plasma, shear, laser-cut or sawn)
CompositionC
≤ 0,12 %
Cr
min. 6,00 % / max. 8,00 %
Al
min. 0,50 % / max. 1,00 %
Scopesengineering
furnace construction
apparatus engineering for high temperature applications
chain industry
Featuresscale resistant up to 800 °C
resistant to oxidizing sulphurous gases
resistant to carburization
only conditionally weldable
good malleability and machinability
corrosion resistant up to 800°C
filler metals: 1.4551, 1.4716, 1.4723, 1.4820, 1.4829
suitable for cold forming as well as hammer and die forging
|
|||||||
1.4724 | X10CrAlSi13 | 405 | X10CrAlSi13 | Z 10 C 13 | 10Ch13SJu | ||
ProductsStrips / foils
Sheets / plates
Pipes
Pipe fittings
Round blanks / rings
Bars
Drawing profiles
Cuts (waterjet, plasma, shear, laser-cut or sawn)
CompositionC
≤ 0,12 %
Si
min. 0,70 % / max. 1,40 %
Mn
≤ 1,00 %
P
≤ 0,04 %
S
≤ 0,015 %
Cr
min. 12,0 % / max. 14,0 %
Al
min. 0,70 % / max. 1,20 %
Scopesengineering
furnace construction
chain industry
grids
high temperature conveyor systems
nozzles for high temperature applications
Featuresresistant to oxidizing sulphurous gases
scale resistant up to 850 °C
good machinability
filler metals: 1.4502, 1.4723, 1.4773, 1.4820, 1.4829
low resistance against carburizing and nitrogen-containing, oxygen-depleted gases
suitable for cold forming as well as hammer and die forging
|
|||||||
1.4742 | X10CrSiAl18-1-1 | 442 | Sicromal 10 | X10CrAlSi18 | Z 10 CAS 18 | 15Ch18SJu | |
ProductsStrips / foils
Sheets / plates
Pipes
Pipe fittings
Round blanks / rings
Bars
Cuts (waterjet, plasma, shear, laser-cut or sawn)
CompositionC
≤ 0,12 %
Si
min. 0,70 % / max. 1,40 %
Cr
min. 17,0 % / max. 19,0 %
Al
min. 0,70 % / max. 1,20 %
Scopesengineering
furnace construction
cement industry
grids
high temperature conveyor systems
nozzles for high temperature applications
power plant technology
heat treatment equipment
Featuresmedium resistance to carburizing and nitrogen-containing, oxygen-depleted gases
resistant to oxidizing sulphurous gases
only conditionally weldable
scale resistant in air from 800-1000 °C
highly malleable
suitable for cold forming as well as hammer and die forging
|
|||||||
1.4762 | X10CrAlSi25 | 446 | S44600, Sicromal 12 | X10CrAlSi25 | Z10CAS24 | ||
ProductsStrips / foils
Sheets / plates
Pipes
Pipe fittings
Round blanks / rings
Bars
Cuts (waterjet, plasma, shear, laser-cut or sawn)
CompositionC
≤ 0,12 %
Si
min. 0,70 % / max. 1,40 %
Mn
≤ 1,00 %
P
≤ 0,04 %
S
[≤ 0,015 %
Cr
min. 23,0 % / max. 26,0 %
Al
min. 1,20 % / max. 1,70 %
Scopessteam boiler
industrial furnace construction
Featuresscale resistant up to 1150 °C
resistant to oxidizing sulphurous gases
filler metals: 1.4773, 1.4822, 1.4842
|
|||||||
1.4828 | X15CrNiSi20-12 | 309S | S30900 | 309 S 24 | Z 17 CNS 20-12 | 20Ch20N14S2 | |
ProductsStrips / foils
Sheets / plates
Pipes
Pipe fittings
Round blanks / rings
Forgings
Bars
Cuts (waterjet, plasma, shear, laser-cut or sawn)
Drawing profiles
CompositionC
max. 0,20 %
Si
min. 1,50 / max. 2,00 %
Cr
min. 19,0 % / max. 21,0 %
Ni
min. 11,0 % / max. 13,0 %
Scopesengineering
furnace construction
automotive industry
chain industry
high temperature components
sieves and grids
Featurescannot be magnetized
medium resistance to carburizing and nitrogen-containing, oxygen-depleted gases
scale resistant in air up to 1000 °C
low corrosion resistance
good machinability, weldability and malleability
suitable for hammer and die forging, cold forming and cold heading
resistant to oxidizing and reducing sulphur-containing gases
high tensile strength at elevated temperatures
weldable with all common procedures
filler metals: 1.4829, 1.4842
|
|||||||
1.4833 | X12CrNi23-13 | 309 | S30900 | 309 S 24 | Z 15 CN 23-13 | ||
ProductsStrips / foils
Sheets / plates
Pipes
Pipe fittings
Round blanks / rings
Bars
Drawing profiles
Cuts (waterjet, plasma, shear, laser-cut or sawn)
CompositionC
≤ 0,15 %
Si
≤ 1,00 %
Mn
≤ 2,00 %
P
≤ 0,045 %
S
≤ 0,015 %
Cr
min. 22,0 % / max. 24,0 %
N
≤ 0,11 %
Ni
min. 12,0 % / max. 14,0 %
Scopesfurnace and apparatus engineering
Featuresfiller metal: 1.4842
scale resistant up to 1000 °C
poor resistance to oxidizing, sulphur-containing gases
|
|||||||
1.4835 | X9CrNiSiNCe21-11-2 | 253MA | S30815 | X9CrNiSiNCe21-11-2 | |||
ProductsStrips / foils
Sheets / plates
Pipes
Pipe fittings
Round blanks / rings
Forgings
Bars
Drawing profiles
Cuts (waterjet, plasma, shear, laser-cut or sawn)
CompositionC
min. 0,05 % / max. 0,12 %
Si
min. 1,40 % / max. 2,50 %
Mn
≤ 1,00 %
P
≤ 0,045 %
S
≤ 0,015 %
Cr
min. 20,0 % / max. 22,0 %
N
min. 0,12 % / max. 0,20 %
Ni
min. 10,0 % / max. 12,0 %
Ce
min. 0,03 % / 0,08 %
Scopesfurnace construction
cement industry
oil installations
heat-treatment equipment for metal industry
hardening plant accessories
apparatus engineering
chain industry
Featuresweldable with all common procedures
filler metal: 1.4842
scale resistant up to 1150 °C
poor resistance to oxidizing gases containing sulphur
high-temperature material
|
|||||||
1.4841 | X15CrNiSi25-21 | 314, 310 | S31000, S31400 | 314 S 25 | Z 15 CNS 25-20 | 20Ch25N20S2 | |
ProductsStrips / foils
Sheets / plates
Profiles
Pipes
Pipe fittings
Round blanks / rings
Forgings
Bars
Drawing profiles
Cuts (waterjet, plasma, shear, laser-cut or sawn)
Scopesengineering
automotive engineering
chemical industry
furnace construction
apparatus engineering for high temperature applications
oil industry
cement industry
Featuresgood strength properties at high temperatures
excellent chemical resistance at temperatures up to 1100 °C
scale resistant in air up to about 1120 °C
exhibits good malleability and weldability
average machinability
suitable for cold forming and cold heading, as well as hammer and die forging
cannot be magnetized
poor resistance to oxidizing and reducing sulphur-containing gases
medium resistance to carburizing and nitrogen-containing, oxygen-depleted gases
weldable with all common welding processes
strong strain hardening
poor thermal conductivity
|
|||||||
1.4845 | X8CrNi25-21 | 310S | S31008 | 310 S 16 | Z 12 CN 26-21 | 08X25H10 | |
ProductsStrips / foils
Sheets / plates
Pipes
Pipe fittings
Round blanks / rings
Forgings
Bars
Drawing profiles
Cuts (waterjet, plasma, shear, laser-cut or sawn)
CompositionC
≤ 0,10 %
Si
≤ 1,50 %
Mn
≤ 2,00 %
P
≤ 0,045 %
S
≤ 0,015 %
Cr
≤ 24,0-26,0 %
Ni
≤ 19,0-22,0 %
N
≤ 0,11 %
Scopesfurnace and apparatus engineering
fasteners for masonry exposed to extreme temperatures
charging baskets
exhaust systems
heating elements
nuts and bolts
heat-resistant chains
Featuressimilar to 1.4841, but with increased toughness
good creep strength
good resistance to high temperature corrosion
scale resistant up to 1050°C
filler metal: 1.4842
machinability is in the range of values for austenitic chromium-nickel steels
weldable with all common procedures, except gas shielded welding
|
|||||||
1.4876 / 1.4958 | X10NiCrAlTi32-20 / X5NiCrAlTi31-20 | 800H, 800H/HT | N08800, N08810, N08811 | NA 15 | Z 10 NC 32-21 / Z 8 NC 33-21 | ||
ProductsStrips / foils
Sheets / plates
Pipes
Pipe fittings
Round blanks / rings
Forgings
Bars
Drawing profiles
Cuts (waterjet, plasma, shear, laser-cut or sawn)
CompositionC
min. 0,06 % / max. 0,08 %
Si
min. 0,2 % / max. 0,6 %
Mn
min. 0,5 % / max. 1,0 %
P
≤ 0,015 %
S
≤ 0,01 %
Cr
min. 19,0 % / max. 21,0 %
Cu
≤ 0,50 %
Ni
min. 30,0 % / max. 32,0 %
Al
min. 0,2 % / max. 0,4 %
Ti
min. 0,2 % / max. 0,5 %
Scopesheat exchanger in coal gasification plants
steam generator tubes in helium-cooled high-temperature reactors
petrochemistry
components for the power plant industry
parts for use in hydrogen generation
Featuresmetallurgical stability in long-term use at high temperatures
good creep strength at temperatures above 600 °C
good resistance in oxidizing, reducing and nitriding atmospheres, and under varying oxidizing and carburizing conditions
filler metals: 2.4806, 2.4648
weldable with all common welding processes
|
All information is supplied without liability reg. e.g. mistakes, completeness or topicality.