Request form

Do you have any queries, want more information or are looking for a product? We´re looking forward to your request!

DELTA-TRADING GmbH Metallhandel

We deliver what you need


The focus of our product range is on special stainless steels, duplex and super duplex grades, special aluminium and heavy metal alloys as well as special materials. We specialise in finding the right solution for you, even for unusual requirements. So you always get what you need, even as a combined package solution depending on your requirements and on request.

We also provide quick and individual processing of materials, from simple drilling to complex laser cutting. This means we can guarantee you get exactly what you need for each of your projects. Punctual, reliable and always in close cooperation with you.

Products

M.-nr. / EN DIN AISI UNS BS AFNOR GOST
1.4000 X6Cr13 410S S41008 403 S 17 X6Cr13 08X13
Products
Strips / foils
Sheets / plates
Round blanks / rings
Drawing profiles
Forgings
Composition
Scopes
oil industry
hydraulic turbines
Features
highly resistant against hydrogen and sulphur
highly weldable with TIG and arc welding
filler metals 1.4009 + 1.4302, etc.
not resistant against intergranular corrosion
high resistance against corrosion in mirror polished or grinded condition
1.4003 X2Cr11 3Cr12 S40977 X2CrNi12 X2CrNi12
Products
Sheets / plates
Pipes
Pipe fittings
Round blanks / rings
Forgings
Drawing profiles
Cuts (waterjet, plasma, shear, laser-cut or sawn)
Composition
C
≤ 0,03 %
Cr
min. 10,5 % / max. 12,5 %
Ni
min. 0,30 % / max. 1,0 %
Scopes
construction industry
engineering
oil industry
automotive industry
mining industry
electronic equipment
transport industry
sugar industry
Features
good machinability
suited for use in mildly corrosive media
higher strengths than other ferrites, can be welded in thicker areas
cold heading grades
use at low temperatures
resistant to wet abrasion
limited use in temp. below 350°C
weldable, except oxyacetylene welding
filler metals: 1.4316 or 1.4370
1.4006 X12Cr13 410 410S21 Z10C13 / Z13C13 12X13
Products
Strips / foils
Sheets / plates
Round blanks / rings
Forgings
Bars
Drawing profiles
Cuts (waterjet, plasma, shear, laser-cut or sawn)
Composition
Cr
min. 0,08 % / max. 0,15 %
Cr
min. 11,50 % / max. 13,50 %
Scopes
oil industry
petrochemical industry
decorative and kitchen equipment
pump industry
hydraulic engineering
Features
ferromagnetic grade
good corrosion resistance in moderately aggressive media (soap, solvents and organic acids)
low susceptibility against embrittlement
good resistance in oxidizing atmospheres up to 600°C
available in annealed and tempered state
before welding. normally preheat to 100-300°C and temper after welding
1.4034 X46Cr13 420 S42000 420S45 Z44C14 / Z38C13 46X13
Products
Strips / foils
Sheets / plates
Round blanks / rings
Forgings
Bars
Drawing profiles
Cuts (waterjet, plasma, shear, laser-cut or sawn)
Composition
C
min. 0,43 % / max. 0,50 %
S
≤ 0,03 %
Cr
min. 12,50 % / max. 14,50 %
Scopes
engineering
medical and pharmaceutical industry
cutlery industry
rolling bearing industry
Features
good corrosion resistance against water and water vapour
not resistant against intergranular corrosion in delivered state
best corrosion resistance in tempered state with polished surface
in general, do not weld 1.4034
good corrosion- resistance in moderately aggressive media (soap, solvents and organic acids)
1.4112 X90CrMoV18 440B
Products
Strips / foils
Sheets / plates
Round blanks / rings
Forgings
Bars
Drawing profiles
Cuts (waterjet, plasma, shear, laser-cut or sawn)
Composition
C
≤ 0,90 %
Cr
≤ 18,0 %
Mo
≤ 1,10 %
V
≤ 0,10
Scopes
cutlery industry
perforated discs
screw elements
bearings
spray nozzle
hardened valves
Features
high tempering ability
wear-resistant
polishable
extremely high edge retention
1.4122 X39CrMo17-1
Products
Strips / foils
Sheets / plates
Round blanks / rings
Forgings
Bars
Drawing profiles
Cuts (waterjet, plasma, shear, laser-cut or sawn)
Composition
C
min. 0,33 % / max. 0,45 %
Cr
min. 15,5 % / max. 17,5 %
Mo
min. 0,80 % / max. 1,30 %
Ni
≤ 1,00 %
Scopes
construction industry
engineering
automotive industry
cutlery industry
food industry
pump shafts
Features
ferromagnetic grade
high gloss polishable
good corrosion resistance in mildly aggressive media and low chlorine ion concentration
without cathodic protection not seawater resistant
better corrosion resistance with polished or finely grinded surfaces
mechanical properties can be improved through annealing
usually not weldable
1.4313 X3CrNiMo13-4 F6NM430 J91540 425 C 11 Z 6 CN 13-04 03X13H4M
Products
Sheets / plates
Round blanks / rings
Forgings
Bars
Cuts (waterjet, plasma, shear, laser-cut or sawn)
Drawing profiles
Composition
C
≤ 0,05 %
Cr
min. 12,0 % / max. 14,0 %
Mo
min. 0,30 % / max. 0,70 %
Ni
min. 3,5 % / max. 4,5 %
N
min. 0,02 %
Scopes
oil industry
petrochemical industry
pump and compressor elements
turbines for water works
tools for casting
Features
ferromagnetic grade
superb mechanical properties
preheat work piece for welding to about 150°C
good corrosion resistance in moderate corrosion environments with no chlorides
much better corrosion resistance with polished surface
optimum processing properties after solution heat treatment at 600-650°C followed by slow cool down
slowly heat work piece for forging to 850°C, then more quickly to 1100-1150°C. Forging at 900-1150°C
machining depends on hardness and strength
1.4362 X2CrNiN23-4 S32304 Z 2 CN 23-04AZ
Products
Strips / foils
Sheets / plates
Pipes
Round blanks / rings
Forgings
Drawing profiles
Cuts (waterjet, plasma, shear, laser-cut or sawn)
Composition
C
≤ 0,03 %
Cr
min. 22,0 % / max. 24,0 %
Mo
min. 0,10 % / max. 0,60 %
Ni
min. 3,5 % / max. 5,5 %
N
min. 0,05 % / max. 0,20 %
Cu
min. 0,10 % / max. 0,60 %
Scopes
construction industry
oil industry
chemical + petrochemical industry
shipbuilding and engineering
Features
weldable
duplex, magnetisable
to be used at -50-300°C
not sensitive to intergranular corrosion
superb resistance against stress corrosion
not polishable
only conditionally machinable
1.4410 X2CrNiMoN25-7-4 F53 S32750 X2CrNiMoN25-7-4 Z 3 CND 25.07Az X2CrNiMoN25-7-4
Products
Strips / foils
Sheets / plates
Hollow steel
Pipes
Pipe fittings
Round blanks / rings
Forgings
Bars
Cuts (waterjet, plasma, shear, laser-cut or sawn)
Drawing profiles
Composition
C
≤ 0,03 %
Si
≤ 0,80 %
Mn
≤ 1,20 %
P
≤ 0,035 %
S
≤ 0,015 %
Cr
min. 24,0 % / max. 26,0 %
Mo
min. 3,0 % / max. 4,5 %
Ni
min. 6,0 % / max. 8,0 %
N
min. 0,24 % / max. 0,35 %
Cu
≤ 0,50 %
Scopes
offshore
desalination plants
piping construction
chemical + petrochemical industry
apparatus and container engineering
chemical tanks
Features
duplex, magnetisable
superb resistance in contact with chloride-containing media
weldable (except gas welding)
excellent corrosion resistance
1.4418 X4CrNiMo16-5-1 S165M X4CrNiMo16-5-1 Z 6 CND 16-05-01
Products
Sheets / plates
Round blanks / rings
Forgings
Bars
Cuts (waterjet, plasma, shear, laser-cut or sawn)
Drawing profiles
Composition
C
≤ 0,06 %
Cr
min. 15,0 % / max. 17,0 %
Mo
min. 0,80 % / max. 1,50 %
Ni
min. 4,0 % / max. 6,0 %
N
min. 0,02 %
Scopes
engineering
chemical industry
shipbuilding
automotive industry (exhaust system)
aerospace industry
Features
superb corrosion resistance in aggressive media
magnetisable
limited use in maritime areas acceptable
extremely resistant against intergranular corrosion
highly resistant against fatigue and stress corrosion
weldable, however work piece preheating to about 100-200°C necessary
suitable for low temperatures
suitable up to 400°C
1.4438 X2CrNiMo18-15-4 317L S31703 317 S 12 X2CrNiMo18-15-4
Products
Strips / foils
Sheets / plates
Profiles
Bars
Drawing profiles
Composition
C
≤ 0,03 %
Si
≤ 1,00 %
Mn
≤ 2,00 %
P
≤ 0,045 %
S
≤ 0,015 %
Cr
min. 17,5 % / max. 19,5 %
Mo
min. 3,00 % / max. 4,00 %
Ni
min. 13,0 % / max. 16,0 %
N
≤ 0,11 %
Paper
Scopes
chemical industry
pulp industry
transport container for chemicals
Features
higher corrosion resistance than AISI 316L, especially in highly corrosive environments with chlorides and halides
filler metals: 1.4440, 1.4438
1.4462 X2CrNiMoN22-5-3 318LN. F51 S31803 318 S 13 Z 2 CND 22-05Az 03X22H5AM3
Products
Strips / foils
Sheets / plates
Hollow steel
Profiles
Pipes
Pipe fittings
Round blanks / rings
Forgings
Bars
Drawing profiles
Cuts (waterjet, plasma, shear, laser-cut or sawn)
Drawing profiles
Composition
C
≤ 0,03 %
Si
≤ 1,00 %
Mn
≤ 2,00 %
P
≤ 0,035 %
S
≤ 0,015 %
Cr
min. 21,0 % / max. 23,0 %
Mo
min. 2,5 % / max. 3,5 %
Ni
min. 4,5 % / max. 6,5 %
N
min. 0,1 % / max. 0,22 %
Scopes
food industry
offshore
desalination plants
paper and pulp industry
chemical and petrochemical industry
desalination plant
nuclear engineering
Features
rust-free austenite, duplex with molybdenum additive, good resistance against pitting and intergranular corrosion
filler metal: 1.4462
temperature range 10-280 °C
hardness / HB30: ≤ 270
1.4501 F55 S32760 X2CrNiMoCuWN25-7-4 Z 3 CND 25.06Az X2CrNiMoCuWN25-7-4
Products
Strips / foils
Sheets / plates
Pipes
Pipe fittings
Round blanks / rings
Forgings
Bars
Cuts (waterjet, plasma, shear, laser-cut or sawn)
Drawing profiles
Composition
C
≤ 0,03 %
Si
≤ 1,00 %
Mn
≤ 1,00 %
P
≤ 0,035 %
S
≤ 0,015 %
Cr
min. 24,0 % / max. 26,0 %
Mo
min. 3,0 % / max. 4,0 %
Ni
min. 6,0 % / max. 8,0 %
N
min. 0,20 % / max. 0,30 %
Cu
min. 0,50 % / max. 1,00 %
W
min. 0,50 % / max. 1,00 %
Fe
Bal.
Scopes
chemical industry
petrochemistry
offshore
desalination plants
container construction
piping construction
chemical tanker construction
Features
duplex
superb corrosion resistance in chloride containing media
weldable (except gas welding)
machining properties comparable with material 1.4462
polishable, but modified appearance of the polishing result is to be expected due to the two-phase structure
good resistance against surface-wide corrosion
comparable to common austenite grades, improved resistance against pitting and crevice corrosion
1.4539 X1NiCrMoCu25-20-5 904L N08904 904 S 13 Z2NCDU25-20
Products
Strips / foils
Sheets / plates
Hollow steel
Pipes
Pipe fittings
Round blanks / rings
Forgings
Bars
Cuts (waterjet, plasma, shear, laser-cut or sawn)
Drawing profiles
Composition
C
≤ 0,02 %
Si
≤ 0,70 %
Mn
≤ 2,0 %
P
≤ 0,03 %
S
≤ 0,01 %
Cr
min. 19,0 % / max. 21,0 %
Mo
min. 4,0 % / max. 5,0 %
Ni
min. 24,0 % / max. 26,0 %
N
≤ 0,15 %
Cu
min. 1,20 % / max. 2,0 %
Scopes
chemical industry
refinery
offshore
paper and pulp industry
seawater technology
Features
excellent resistance against intergranular corrosion, stress corrosion and pitting
filler metals: 1.4539, 1.4519
1.4547 X1CrNiMoCuN20-18-7 254SMO S31254 X1CrNiMoCuN20-18-7 X1CrNiMoCuN20-18-7
Products
Strips / foils
Sheets / plates
Pipes
Round blanks / rings
Forgings
Bars
Cuts (waterjet, plasma, shear, laser-cut or sawn)
Drawing profiles
Composition
C
≤ 0,02 %
Si
≤ 0,70 %
Mn
≤ 1,00 %
P
≤ 0,03 %
S
≤ 0,01 %
Cr
min. 19,5 % / max. 20,5 %
Mo
min. 6,0 % / max. 7,0 %
Ni
min. 17,5 % / max. 18,5 %
N
min. 0,18 % / max. 0,25 %
Cu
min. 0,50 % / max. 1,0 %
Fe
Rest
Scopes
shipbuilding
offshore
desalination plants
paper and pulp industry
water treatment plants
Features
weldable
machinable in annealed condition
tends towards strain hardening
excellent resistance against pitting, crevice corrosion and surface erosion
cannot be magnetized in solution annealed condition
cannot be cured by heat treatment
seawater resistant
1.4550 X6CrNiNb18-10 347, 347H S34700 347 S 20 X6CrNiNb18-10 08Ch18N12B
Products
Strips / foils
Sheets / plates
Pipes
Pipe fittings
Round blanks / rings
Forgings
Bars
Drawing profiles
Cuts (waterjet, plasma, shear, laser-cut or sawn)
Composition
C
≤ 0,08 %
Si
≤ 1,00 %
Mn
≤ 2,00 %
P
≤ 0,045 %
S
≤ 0,015 %
Cr
min. 17,0 % / max. 19,0 %
Nb
10 x C
Ni
min. 9,00 % / max. 12,0 %
Scopes
food industry
chemical industry
Features
good resistance against intergranular corrosion
filler metals: 1.4316, 1.4551, 1.4576
1.4713 X10CrAl7 Sicromal 8 X10CrAlSi7 12X7CIO
Products
Strips / foils
Sheets / plates
Pipes
Round blanks / rings
Bars
Drawing profiles
Cuts (waterjet, plasma, shear, laser-cut or sawn)
Composition
C
≤ 0,12 %
Cr
min. 6,00 % / max. 8,00 %
Al
min. 0,50 % / max. 1,00 %
Scopes
engineering
furnace construction
apparatus engineering for high temperature applications
chain industry
Features
scale resistant up to 800 °C
resistant to oxidizing sulphurous gases
resistant to carburization
only conditionally weldable
good malleability and machinability
corrosion resistant up to 800°C
filler metals: 1.4551, 1.4716, 1.4723, 1.4820, 1.4829
suitable for cold forming as well as hammer and die forging
1.4724 X10CrAlSi13 405 X10CrAlSi13 Z 10 C 13 10Ch13SJu
Products
Strips / foils
Sheets / plates
Pipes
Pipe fittings
Round blanks / rings
Bars
Drawing profiles
Cuts (waterjet, plasma, shear, laser-cut or sawn)
Composition
C
≤ 0,12 %
Si
min. 0,70 % / max. 1,40 %
Mn
≤ 1,00 %
P
≤ 0,04 %
S
≤ 0,015 %
Cr
min. 12,0 % / max. 14,0 %
Al
min. 0,70 % / max. 1,20 %
Scopes
engineering
furnace construction
chain industry
grids
high temperature conveyor systems
nozzles for high temperature applications
Features
resistant to oxidizing sulphurous gases
scale resistant up to 850 °C
good machinability
filler metals: 1.4502, 1.4723, 1.4773, 1.4820, 1.4829
low resistance against carburizing and nitrogen-containing, oxygen-depleted gases
suitable for cold forming as well as hammer and die forging
1.4742 X10CrSiAl18-1-1 442 Sicromal 10 X10CrAlSi18 Z 10 CAS 18 15Ch18SJu
Products
Strips / foils
Sheets / plates
Pipes
Pipe fittings
Round blanks / rings
Bars
Cuts (waterjet, plasma, shear, laser-cut or sawn)
Composition
C
≤ 0,12 %
Si
min. 0,70 % / max. 1,40 %
Cr
min. 17,0 % / max. 19,0 %
Al
min. 0,70 % / max. 1,20 %
Scopes
engineering
furnace construction
cement industry
grids
high temperature conveyor systems
nozzles for high temperature applications
power plant technology
heat treatment equipment
Features
medium resistance to carburizing and nitrogen-containing, oxygen-depleted gases
resistant to oxidizing sulphurous gases
only conditionally weldable
scale resistant in air from 800-1000 °C
highly malleable
suitable for cold forming as well as hammer and die forging
1.4762 X10CrAlSi25 446 S44600, Sicromal 12 X10CrAlSi25 Z10CAS24
Products
Strips / foils
Sheets / plates
Pipes
Pipe fittings
Round blanks / rings
Bars
Cuts (waterjet, plasma, shear, laser-cut or sawn)
Composition
C
≤ 0,12 %
Si
min. 0,70 % / max. 1,40 %
Mn
≤ 1,00 %
P
≤ 0,04 %
S
[≤ 0,015 %
Cr
min. 23,0 % / max. 26,0 %
Al
min. 1,20 % / max. 1,70 %
Scopes
steam boiler
industrial furnace construction
Features
scale resistant up to 1150 °C
resistant to oxidizing sulphurous gases
filler metals: 1.4773, 1.4822, 1.4842
1.4828 X15CrNiSi20-12 309S S30900 309 S 24 Z 17 CNS 20-12 20Ch20N14S2
Products
Strips / foils
Sheets / plates
Pipes
Pipe fittings
Round blanks / rings
Forgings
Bars
Cuts (waterjet, plasma, shear, laser-cut or sawn)
Drawing profiles
Composition
C
max. 0,20 %
Si
min. 1,50 / max. 2,00 %
Cr
min. 19,0 % / max. 21,0 %
Ni
min. 11,0 % / max. 13,0 %
Scopes
engineering
furnace construction
automotive industry
chain industry
high temperature components
sieves and grids
Features
cannot be magnetized
medium resistance to carburizing and nitrogen-containing, oxygen-depleted gases
scale resistant in air up to 1000 °C
low corrosion resistance
good machinability, weldability and malleability
suitable for hammer and die forging, cold forming and cold heading
resistant to oxidizing and reducing sulphur-containing gases
high tensile strength at elevated temperatures
weldable with all common procedures
filler metals: 1.4829, 1.4842
1.4833 X12CrNi23-13 309 S30900 309 S 24 Z 15 CN 23-13
Products
Strips / foils
Sheets / plates
Pipes
Pipe fittings
Round blanks / rings
Bars
Drawing profiles
Cuts (waterjet, plasma, shear, laser-cut or sawn)
Composition
C
≤ 0,15 %
Si
≤ 1,00 %
Mn
≤ 2,00 %
P
≤ 0,045 %
S
≤ 0,015 %
Cr
min. 22,0 % / max. 24,0 %
N
≤ 0,11 %
Ni
min. 12,0 % / max. 14,0 %
Scopes
furnace and apparatus engineering
Features
filler metal: 1.4842
scale resistant up to 1000 °C
poor resistance to oxidizing, sulphur-containing gases
1.4835 X9CrNiSiNCe21-11-2 253MA S30815 X9CrNiSiNCe21-11-2
Products
Strips / foils
Sheets / plates
Pipes
Pipe fittings
Round blanks / rings
Forgings
Bars
Drawing profiles
Cuts (waterjet, plasma, shear, laser-cut or sawn)
Composition
C
min. 0,05 % / max. 0,12 %
Si
min. 1,40 % / max. 2,50 %
Mn
≤ 1,00 %
P
≤ 0,045 %
S
≤ 0,015 %
Cr
min. 20,0 % / max. 22,0 %
N
min. 0,12 % / max. 0,20 %
Ni
min. 10,0 % / max. 12,0 %
Ce
min. 0,03 % / 0,08 %
Scopes
furnace construction
cement industry
oil installations
heat-treatment equipment for metal industry
hardening plant accessories
apparatus engineering
chain industry
Features
weldable with all common procedures
filler metal: 1.4842
scale resistant up to 1150 °C
poor resistance to oxidizing gases containing sulphur
high-temperature material
1.4841 X15CrNiSi25-21 314, 310 S31000, S31400 314 S 25 Z 15 CNS 25-20 20Ch25N20S2
Products
Strips / foils
Sheets / plates
Profiles
Pipes
Pipe fittings
Round blanks / rings
Forgings
Bars
Drawing profiles
Cuts (waterjet, plasma, shear, laser-cut or sawn)
Composition
C
≤ 0,20 %
Si
≤ 1,50-2,50 %
Cr
≤ 24,0-26,0 %
Ni
≤ 19,0-22,0 %
Paper
Scopes
engineering
automotive engineering
chemical industry
furnace construction
apparatus engineering for high temperature applications
oil industry
cement industry
Features
good strength properties at high temperatures
excellent chemical resistance at temperatures up to 1100 °C
scale resistant in air up to about 1120 °C
exhibits good malleability and weldability
average machinability
suitable for cold forming and cold heading, as well as hammer and die forging
cannot be magnetized
poor resistance to oxidizing and reducing sulphur-containing gases
medium resistance to carburizing and nitrogen-containing, oxygen-depleted gases
weldable with all common welding processes
strong strain hardening
poor thermal conductivity
1.4845 X8CrNi25-21 310S S31008 310 S 16 Z 12 CN 26-21 08X25H10
Products
Strips / foils
Sheets / plates
Pipes
Pipe fittings
Round blanks / rings
Forgings
Bars
Drawing profiles
Cuts (waterjet, plasma, shear, laser-cut or sawn)
Composition
C
≤ 0,10 %
Si
≤ 1,50 %
Mn
≤ 2,00 %
P
≤ 0,045 %
S
≤ 0,015 %
Cr
≤ 24,0-26,0 %
Ni
≤ 19,0-22,0 %
N
≤ 0,11 %
Scopes
furnace and apparatus engineering
fasteners for masonry exposed to extreme temperatures
charging baskets
exhaust systems
heating elements
nuts and bolts
heat-resistant chains
Features
similar to 1.4841, but with increased toughness
good creep strength
good resistance to high temperature corrosion
scale resistant up to 1050°C
filler metal: 1.4842
machinability is in the range of values for austenitic chromium-nickel steels
weldable with all common procedures, except gas shielded welding
1.4876 / 1.4958 X10NiCrAlTi32-20 / X5NiCrAlTi31-20 800H, 800H/HT N08800, N08810, N08811 NA 15 Z 10 NC 32-21 / Z 8 NC 33-21
Products
Strips / foils
Sheets / plates
Pipes
Pipe fittings
Round blanks / rings
Forgings
Bars
Drawing profiles
Cuts (waterjet, plasma, shear, laser-cut or sawn)
Composition
C
min. 0,06 % / max. 0,08 %
Si
min. 0,2 % / max. 0,6 %
Mn
min. 0,5 % / max. 1,0 %
P
≤ 0,015 %
S
≤ 0,01 %
Cr
min. 19,0 % / max. 21,0 %
Cu
≤ 0,50 %
Ni
min. 30,0 % / max. 32,0 %
Al
min. 0,2 % / max. 0,4 %
Ti
min. 0,2 % / max. 0,5 %
Scopes
heat exchanger in coal gasification plants
steam generator tubes in helium-cooled high-temperature reactors
petrochemistry
components for the power plant industry
parts for use in hydrogen generation
Features
metallurgical stability in long-term use at high temperatures
good creep strength at temperatures above 600 °C
good resistance in oxidizing, reducing and nitriding atmospheres, and under varying oxidizing and carburizing conditions
filler metals: 2.4806, 2.4648
weldable with all common welding processes
2.4360 (Alloy 400) NiCu30Fe N04400 NA13 Nu30
Products
Sheets / plates
Pipes
Pipe fittings
Cuts (waterjet, plasma, shear, laser-cut or sawn)
Composition
C
≤ 0,15 %
Si
≤ 0,50 %
Mn
≤ 2,00 %
Ti
≤ 0,30 %
Ti
≤ 0,30 %
S
≤ 0,02 %
Al
≤ 0,50 %
Cu
min. 28,0 % / max. 34,0 %
Ni
≤ 63,00 %
Fe
min. 1,0 % / max. 2,5 %
Scopes
chemical industry
apparatus engineering
refinery
pipes for sulphuric acid
wastewater treatment
seawater desalination
pressure container construction
Features
heat resistant
chemically resistant
seawater resistant
filler metal: 2.4366
good toughness and strength
largely insensitive to stress corrosion
suitable for cold and heat forming
2.4668 (Alloy 718) NiCr19NbMo N07718
Products
Sheets / plates
Pipes
Round blanks / rings
Bars
Composition
C
min. 0,02 % / max. 0,08 %
Si
≤ 0,35 %
Mn
≤ 0,35 %
P
≤ 0,015 %
S
≤ 0,015 %
Cr
min. 17,0 % / max. 21,0 %
Mo
min. 2,80 % / max. 3,30 %
Ni
min. 50,0 % / max. 55,0 %
Ti
min. 0,60 % / max. 1,20 %
Cu
≤ 0,30 %
Al
min. 0,30 % / max. 0,70 %
Nb
min. 4,70 % / max. 5,50 %
Co
≤ 1,00 %
B
min. 0,002 % / max. 0,006 %
Fe
Rest
Scopes
offshore + marine engineering equipment
aviation and aerospace
nuclear reactors
springs
high-strength bolts
oil and gas industry
Features
very good mechanical properties at low to very low temperatures
excellent corrosion resistance at high and low temperatures
filler metal: 2.4667
very good creep strength
high fatigue strength
highly weldable (arc and resistance welding methods)
curable by heat treatment
2.4819 (Alloy C-276) NiMo16Cr15W N10276
Products
Strips / foils
Sheets / plates
Pipes
Round blanks / rings
Bars
Cuts (waterjet, plasma, shear, laser-cut or sawn)
Composition
C
≤ 0,01 %
Si
≤ 0,08 %
Mn
≤ 1,00 %
P
≤ 0,025 %
S
≤ 0,010 %
Cr
min. 14,5 % / max. 16,5 %
Mo
min. 15,0 % / max. 17,0 %
Ni
Rest
V
≤ 0,35 %
W
min. 3,0 % / max. 4,5 %
Co
≤ 2,50 %
Scopes
pulp industry
refuse incineration plant
flue gas desulfurization system
petroleum and natural gas
chemical engineering
Features
suitable for cold and heat forming
excellent resistance to oxidizing and reducing media, even at elevated temperatures
high resistance to crevice corrosion, pitting and stress corrosion cracking in oxidizing and reducing media
good resistance to a variety of corrosive media, incl. strong oxidants such as iron (III) chloride and copper (II) chloride, hot media
good resistance in moist chlorine gas, sodium chloride and chlorine dioxide
weldable with all common welding processes
2.4856 (Alloy 625) NiCr22Mo9Nb Alloy 625 N06625
Products
Sheets / plates
Pipes
Pipe fittings
Round blanks / rings
Bars
Composition
C
min. 0,03 % / max. 0,10 %
Si
≤ 0,50 %
Mn
≤ 0,50 %
P
≤ 0,02 %
S
≤ 0,015 %
Cr
min. 20,0 % / max. 23,0 %
Mo
min. 8,00 % / max. 10,0 %
Ni
≤ 58,00 %
Ti
≤ 0,40 %
Cu
≤ 0,50 %
Al
≤ 0,40 %
Co
≤ 1,00 %
Fe
≤ 5,00 %
Nb
min. 3,15 % / max. 4,15 %
Scopes
chemical industry
offshore technology
environmental engineering
flue gas cleaning systems
installations for the extraction of natural gas and oil
Features
suitable for cold and heat forming
exceptional resistance to pitting, crevice corrosion, erosion and intergranular corrosion
good resistance to mineral acids
good resistance to alkalis and organic acids
filler metals: 2.4831, 2.4621
excellent high temperature strength and wear properties
good resistance to oxidation and carburizing
TIG, MIG and arc welding processes
3.0255 / EN AW 1050
Products
H111, H12, H14, H18, H22, H24, H26, H28
Dichte: 2,71
Composition
Scopes
food industry
chemical industry
apparatus and container engineering
Features
3.0275/ EN AW 1070
Products
H111, H12, H14, H18, H22, H24, H26, H28
Dichte: 2,71
Composition
Scopes
electrical engineering
medical and pharmaceutical industry
food industry
vehicle construction
Features
high corrosion resistance
3.0505 / EN AW-3105 AlMn0,5Mg0,5
Products
Strips / foils
Sheets / plates
Pipes
Material condition: H14, H24, H16, H26, H18, H28 Density: 2,7
Composition
Si
≤ 0,60 %
Fe
≤ 0,70 %
Cu
≤ 0,30 %
Mn
min. 0,30 % / max. 0,80 %
Mg
min. 0,20 % / max. 0,80 %
Cr
≤ 0,20 %
Zn
≤ 0,40 %
Ti
≤ 0,10 %
Scopes
automotive engineering
vehicle construction
air conditioning systems
white goods
ventilation systems
Features
excellent corrosion resistance
good forming properties
3.0506 / EN AW 5005
Products
H111, H12, H14, H18, H22, H24, H26, H28 Dichte: 2,71
Composition
Scopes
façade engineering
Features
medium strength
high corrosion resistance
3.0515 / EN AW-3003 AlMn1Cu
Products
Strips / foils
Sheets / plates
Pipes
Material condition: 0,H111, H112, H14, H24, H18 Density: 2,73
Composition
Si
≤ 0,50 %
Fe
≤ 0,70 %
Cu
≤ 0,10
Mn
min. 0,90 % / max. 1,50 %
Mg
≤ 0,30 %
Cr
≤ 0,10 %
Zn
≤ 0,20 %
Ti
≤ 0,10 %
Sonstige
≤ 0,05 %
Scopes
roofing
claddings
vehicle construction, container and apparatus engineering
cans
rigid film containers
Features
weldable
medium strength
high corrosion resistance
very good forming properties
3.0515 / EN AW-3103 AlMn1Cu
Products
Strips / foils
Sheets / plates
Pipes
Material condition: 0, H111, H112, H24, H11-H18 Density: 2,73
Composition
Si
≤ 0,50 %
Fe
≤ 0,70 %
Cu
≤ 0,10 %
Mn
min. 0,90 % / max. 1,50 %
Mg
≤ 0,30 %
Cr
≤ 0,10 %
Zn
≤ 0,20 %
Zr+Ti
≤ 0,10 %
Scopes
air conditioning systems
white goods
ventilation systems
façade and interiors (coated sheets)
Features
excellent corrosion resistance
good forming properties
3.0525 / EN AW-3005 AlMn1Mg0,5
Products
Strips / foils
Sheets / plates
Pipes
Material condition: H14, H24, H16, H26, H18, H28 Density: 2,7
Composition
Si
≤ 0,60 %
Fe
≤ 0,70 %
Cu
≤ 0,30 %
Mn
min. 1,0 % / max. 1,5 %
Mg
min. 0,2 % / max. 0,6 %
Cr
≤ 0,10 %
Zn
≤ 0,25 %
Ti
≤ 0,10 %
Scopes
ladders
all types of flashings
roofing and cladding
aerials
staircases
roller shutters
heat insulation
Features
very good corrosion resistance
good mechanical properties
highly weldable and good forming properties
3.1255 / EN AW-2014 AlCuSiMn
Products
Strips / foils
Sheets / plates
Profiles
Pipes
Forgings
Material condition: T3, T6
Composition
Si
min. 0,5 % / max. 0,9 %
Fe
≤ 0,50 %
Cu
min. 3,9 % / max. 5,0 %
Mn
min. 0,4 % / max. 1,2 %
Mg
min. 0,2 % / max. 0,8 %
Cr
≤ 0,10 %
Ni
≤ 0,10 %
Zn
≤ 0,25 %
Ti
≤ 0,15 %
Scopes
aerospace components
military vehicles
bridge and building constructions
Features
highly machinable in cured condition
not suitable for soldering, except abrasion soldering
suitable for protective anodizing + coating
slightly weatherproof
no decorative anodized surface
not suitable for welding, except resistance welding
3.1325 / EN AW-2017A AlCuMg1
Products
Strips / foils
Sheets / plates
Profiles
Pipes
Forgings
Material condition: T3, T4510, T4511 Density: 2,80
Composition
Si
min. 0,2 % / max. 0,8 %
Fe
≤ 0,70 %
Cu
min. 3,5 % / max. 4,5 %
Mn
min. 0,4 % / max. 1,0 %
Mg
min. 0,4 % / max. 1,0 %
Cr
≤ 0,10 %
Zn
≤ 0,25 %
Scopes
engineering
aviation
transport and traffic
forgings
Features
good machinability in cured condition
very low corrosion resistance
not suitable for soldering, except abrasion soldering
no decorative anodized surface
not suitable for welding, except resistance welding
suitable for protective anodizing and coating
3.1355 / EN AW-2024 AlCuMg2
Products
Strips / foils
Sheets / plates
Profiles
Pipes
Forgings
Material condition: T3, T3510, T3511 Density: 2,77
Composition
Si
≤ 0,50 %
Fe
≤ 0,50 %
Cu
min. 3,8 % / max. 4,9 %
Mn
min. 0,3 % / max. 0,9 %
Mg
min. 1,2 % / max. 1,8 %
Cr
≤ 0,10 %
Zn
≤ 0,25 %
Ti
≤ 0,15 %
Scopes
engineering
aeronautical engineering
Features
very low corrosion resistance
not suitable for soldering, except abrasion soldering
no decorative anodized surface
not suitable for welding, except resistance welding
suitable for protective anodizing and coating
good machinability in cured and annealed condition
3.1645 / EN AW-2007 AlCuMgPb
Products
Profiles
Pipes
Material condition: T3, T4, T4511 Density: 2,85
Composition
Si
≤ 0,80 %
Fe
≤ 0,80 %
Cu
min. 3,3 % / max. 4,6 %
Mn
min. 0,5 % / max. 1,0 %
Cr
≤ 0,10 %
Ni
≤ 0,20 %
Zn
≤ 0,80 %
Ti
≤ 0,20 %
Pb
≤ 1,5 %
Scopes
most commonly used drilling, turning and milling quality
Features
conditionally suitable for coating
not suitable for anodizing
very high machinability
not suitable for welding
very low corrosion resistance
3.2315 / EN AW-6082 AlMgSi1
Products
Strips / foils
Sheets / plates
Profiles
Pipes
Drawing profiles
Composition
Cu
≤ 0,10 %
Mn
min. 0,40 % / max. 1,0 %
Si
min. 0,7 % / max. 1,3 %
Al
Rest
Zn
≤ 0,20 %
Mg
min. 0,6 % / max. 1,2 %
Fe
≤ 0,50 %
Cr
≤ 0,25 %
Ti
≤ 0,10 %
Sonstige
≤ 0,15 %
Scopes
engineering
electrical engineering
structural elements
pump bodies
shipbuilding
conveyance
Features
highly workable and weldable
very good corrosion resistance
good suitability for anodic oxidation, however suitability for decorative purposes limited
well suited for extrusion, die and hammer forging
superior conductivity
3.3206 / EN AW-6060 AlMgSi0,5
Products
Profiles
Pipes
Pipe fittings
Drawing profiles
Composition
Si
min. 0,30 % / max. 0,60 %
Fe
min. 0,10 % / max. 0,30 %
Cu
≤ 0,10 %
Mn
≤ 0,10 %
Mg
min. 0,35 % / max. 0,60 %
Cr
≤ 0,05 %
Zn
≤ 0,15 %
Ti
≤ 0,10 %
Sonstige
0,15 %
Paper
Scopes
construction industry
engineering
automotive engineering
façade engineering
flagpoles
food industry
medical and rehab (rehabilitation) technology
door and window construction
Features
good cold forming properties when cured
weldable with all common procedures, except resistance welding
very well suited for coating / anodizing, also decorative
good machinability in cured condition
good corrosion resistance, even in seawater
well suited for abrasion and soft soldering and brazing
standard alloy for extrusion profiles
3.3206 / EN AW-6063 AlMgSi0,7
Products
Profiles
Pipes
Drawing profiles
Composition
Cu
≤ 0,10 %
Mn
≤ 0,10 %
Si
min. 0,20 % / max. 0,60 %
Al
Rest
Zn
≤ 0,10 %
Mg
min. 0,45 % / max. 0,90 %
Fe
≤ 0,35 %
Cr
≤ 0,10 %
Ti
≤ 0,10 %
Sonstige
≤ 0,15 %
Scopes
furniture industry
door and window frames
automotive industry
façade construction
flagpoles and lamp posts
Features
good suitability for anodizing, also for decorative purposes
easily weldable, formable and workable
is mainly used as an extruded alloy
3.3211 / EN AW-6061 AlMg1SiCu
Products
Strips / foils
Sheets / plates
Profiles
Pipes
Drawing profiles
Composition
Si
min. 0,40 % / max. 0,80 %
Fe
≤ 0,70 %
Cu
min. 0,15 % / max. 0,40 %
Mn
≤ 0,15 %
Mg
min. 0,80 % / max. 1,20 %
Cr
min. 0,04 % / max. 0,35 %
Zn
≤ 0,25 %
Ti
≤ 0,15 %
Sonstige
0,15 %
Paper
Scopes
construction industry
engineering
ladders
Features
good machinability in cured condition
cold forming properties limited when cured
weldable with all common procedures
well suited for coating / anodizing
good corrosion resistance, fair in seawater
well suited for abrasion soldering and brazing with flux
3.3535 / EN AW 5754
Products
H111, H12, H14, H18, H22, H24, H26, H28
Dichte: 2,71
Composition
Scopes
shipbuilding
apparatus engineering
food industry
vehicle construction
Features
3.4335 / EN AW-7020 AlZn4,5Mg1
Products
Strips / foils
Sheets / plates
Profiles
Pipes
Drawing profiles
Material condition: T6, T62, T651 Density: 2,77
Composition
Si
≤ 0,35 %
Fe
≤ 0,40 %
Cu
≤ 0,20 %
Mn
min. 0,05 % / max. 0,50 %
Mg
min. 1,0 % / max. 1,4 %
Cr
min. 0,10 % / max. 0,35 %
Zn
min. 4,0 % / max. 5,0 %
Zr+Ti
min. 0,08 % / max. 0,25 %
zus
≤ 0,15 %
Scopes
profiles for load carrying systems
welded assemblies with high required tensile strength
Features
good machinability
not suitable for soldering, except abrasion soldering
good machinability in cured and annealed condition
medium corrosion resistance
suitable for protective anodizing and coating
good to excellent weldability, except resistance welding
3.4345 / EN AW-7022 AlZn5Mg3Cu
Products
Strips / foils
Sheets / plates
Profiles
Pipes
Drawing profiles
Material condition: T6, T651 Density: 2,78
Composition
Si
≤ 0,50 %
Fe
≤ 0,50 %
Cu
min. 0,5 % / max. 1,0 %
Mn
min. 0,10 % / max. 0,40 %
Mg
min. 2,6 % / max. 3,7 %
Cr
min. 0,10 % / max. 0,30 %
Zn
min. 4,3 % / max. 5,2 %
Zr+Ti
≤ 0,20 %
zus
≤ 0,15 %
Scopes
toolmaking and mold construction
Features
very low corrosion resistance
suitable for protective anodizing and coating
not solderable
not weldable, except resistance welding
not suitable for cold forming
3.4365 / EN AW-7075 AlZn5,5MgCu
Products
Strips / foils
Sheets / plates
Profiles
Pipes
Drawing profiles
Material condition: T6, T651, T62 Density: 2,80
Composition
Si
≤ 0,40 %
Fe
≤ 0,50 %
Cu
min. 1,2 % / max. 2,0 %
Mn
≤ 0,30 %
Mg
min. 2,1 % / max. 2,9 %
Cr
≤ 0,18-0,28 %
Zn
min. 5,1 % / max. 6,1 %
Ti
≤ 0,20 %
zus
≤ 0,15 %
Scopes
engineering
aviation
special alloy for toolmaking / mold and fixture construction
Features
very good resistance to weather and seawater
not solderable
not suitable for welding, except resistance welding
poor cold forming properties
good machinability
limited suitability for coating, but not for anodizing, except protective anodizing
3.4365x / EN AW-7005 AlZnMg1
Products
Pipes
Drawing profiles
Material condition: T6 Density: 2,77
Composition
Si
≤ 0,35 %
Fe
≤ 0,40 %
Cu
≤ 0,10 %
Mn
min. 0,20 % / max. 0,70 %
Mg
min. 1,0 % / max. 1,8 %
Cr
min. 0,06 % / max. 0,20 %
Zn
min. 4,0 % / max. 5,0 %
Ti
min. 0,01 % / max. 0,06 %
Scopes
frame construction (bicycles)
tent poles
statically stressed constructions
Features
American alloy, equivalent to EN AW-7020
CC331G (2.0940) CuAl10Fe
Products
Round blanks / rings
Forgings
Bars
Density: 7,5
Composition
Al
min. 8,5 % / max. 10,5 %
Ni
≤ 1,5 %
Fe
min. 1,5 % / max. 3,5 %
Mn
≤ 1,0 %
Cu
min. 83,0 % / max. 89,5 %
Si
≤ 0,2 %
Mg
≤ 0,05 %
Pb
≤ 0,1 %
Sn
≤ 0,2 %
Zn
≤ 0,5 %
Scopes
food industry
acid-resistant fittings
Features
high corrosion resistance against seawater and acid
high rigidity
CC483K (2.1052.04) CuSn12-C C90800
Products
Hollow steel
Round blanks / rings
Forgings
Bars
Cuts (waterjet, plasma, shear, laser-cut or sawn)
Density: 8,72
Composition
Cu
min. 85,0 % / max. 88,5 %
Ni
≤ 2,0 %
P
≤ 0,60 %
Pb
≤ 0,70 %
Sn
min. 11,0 % / max. 13,0 %
Al
≤ 0,01 %
Fe
≤ 0,2 %
Mn
≤ 0,2 %
S
≤ 0,05 %
Sb
≤ 0,15 %
Si
≤ 0,01 %
Zn
≤ 0,5 %
Scopes
worm wheels and helical gear
shaft nuts and coupling pieces
worm wheel rims and cylinder inserts
cavitation stressed construction elements
Features
wear resistant, hard and tough
excellent corrosion resistance, especially against seawater
CC493K (2.1090) CuSn7Zn4Pb7-C / RG7 C93200
Products
Hollow steel
Profiles
Pipes
Round blanks / rings
Forgings
Bars
Cuts (waterjet, plasma, shear, laser-cut or sawn)
Density: 8,8
Composition
Cu
min. 81,0 % / max. 85,0 %
Ni
≤ 2,0 %
P
≤ 0,1 %
Pb
min. 5,0 % / max. 8,0 %
Sn
min. 6,0 % / max. 8,0 %
Al
≤ 0,01 %
Fe
≤ 0,2 %
S
≤ 0,10 %
Sb
≤ 0,30 %
Si
≤ 0,01 %
Zn
min. 2,0 % / max. 5,0 %
Scopes
general engineering
toolmaking
small end bushes
setting increment, coupling pieces
propeller shat sleeves
and others
Features
seawater resistant
good machinability
good machinability
medium hard, high wear resistance
good emergency operating properties
good corrosion resistance
poor weldability
suitable for soft and hard soldering
suitable for polishing, galvanizing and dip soldering
CC496K (2.1182) GZ-CuPb15Sn C93900
Products
Hollow steel
Pipes
Round blanks / rings
Forgings
Bars
Density: 9,1
Composition
Cu
min. 74,0 % / max. 80,0 %
Ni
min. 0,5 % / max. 2,0 %
P
≤ 0,1 %
Pb
min. 13,0 % / max. 17,0 %
Sn
min. 6,0 % / max. 8,0 %
Al
≤ 0,01 %
Fe
≤ 0,25 %
Mn
≤ 0,2 %
S
≤ 0,1 %
Sb
≤ 0,5 %
Si
≤ 0,01 %
Zn
≤ 2,0 %
Scopes
engineering
plain bearings
bearings with very high surface pressures
Features
excellent machinability
excellent anti-friction and emergency operating properties
not suitable for temperatures over 120°C
resistant against sulphuric acid
CC762S (2.0598) GZ-CuZn25Al5
Products
Hollow steel
Forgings
Bars
Density: 8,2
Composition
Cu
min. 60,0 % / max. 67,0 %
Ni
≤ 3,0 %
P
≤ 0,03 %
Pb
≤ 0,2 %
Sn
≤ 0,2 %
Al
min. 3,0 % max. 7,0 %
Fe
min. 1,5 % / max. 4,0 %
Mn
min. 2,5 % / max. 5,0 %
Sb
≤ 0,03 %
Si
≤ 0,1 %
Zn
Rest
Scopes
thrust bearing rings
bridge bearings
inner bearings and spindles for high pressure valves
hinged blocks in rolling mills
pressure shell for bloom and slab shears
Features
not solderable
structural material suitable for high static loads
very high yield strength and tensile strength
not suitable for dynamic loads with vibrations
applicable up to max. 150°C
mid-level machinability
very low weldability
CC764S (2.0596) GZ-CuZn34Al2
Products
Hollow steel
Forgings
Bars
Density: 8,6
Composition
Cu
min. 55,0 % / max. 66,0 %
Ni
≤ 3,0 %
P
≤ 0,03 %
Pb
≤ 0,3 %
Sn
≤ 0,3 %
Al
min. 1,0 % / max. 3,0 %
Fe
min. 0,5 / max. 2,5 %
Mn
min. 1,0 % / max. 4,0 %
Sb
≤ 0,05 %
Si
≤ 0,1 %
Zn
Rest
Scopes
compression elements
pressure parts
valve and control parts
Features
seawater resistant
not solderable
very low weldability
hard structural material
high rigidity, medium elongation
very high static resilience
moderate anti-friction properties and poor emergency operating properties
CC765S (2.0592) GZ-CuZn35Al1
Products
Hollow steel
Forgings
Bars
Density: 8,6
Composition
Cu
min. 57,0 % / max. 65,0 %
Ni
≤ 6,0 %
P
≤ 0,03 %
Pb
≤ 0,5 %
Sn
≤ 1,0 %
Al
min. 0,5 / max. 2,5 %
Fe
min. 0,5 / max. 2,0 %
Mn
≤ 0,5-3,0 %
Sb
≤ 0,08 %
Si
≤ 0,1 %
Zn
Rest
Scopes
screw propeller and superstructures
pressure and sliding plates
crane rail wheel sockets
Features
seawater resistant
not solderable
very low weldability
hard and tough structural material
high rigidity and elongation
high static resilience even with stress due to vibration and shock
moderate anti-friction properties and poor emergency operating properties
CW101C (2.2147) CuBe2 C17200
Products
Pipes
Forgings
Bars
Density: 8,3
Composition
Cu
Rest
Ni+Co
> 0,2 %
Be
min. 1,8 % / max. 2,0 %
Ni+Co+Fe
≤ 0,60 %
Pb
≤ 0,10 %
Scopes
mechanically high stressed brackets, holders and strips
non-arcing and non-magnetic safety parts for on-/offshore technology
components for precision measurement devices
high strength and corrosion resistant elements for seawater technology
Features
high corrosion resistance
good electrical conductivity
thermally curable
weldable
cold and heat formable
poor machinability
avoid sulphur-containing coolants and lubricants
hard and soft solderable
CW104C (2.1285) CuCo2Be C17500
Products
Pipes
Forgings
Bars
Density: 8,85
Composition
Cu
Rest
Co
min. 2,0 % / max. 2,8 %
Be
min. 0,4 % / max. 0,7 %
Ni+Fe
≤ 0,5 %
Scopes
open die-forged parts (axis and shafts) for resistance welding technology
Features
good machinability
thermally curable
good tensile strength and high thermal resistance as well as good electrical and thermal conductivity in hardened condition
good heat forming properties
hard and soft solderable
weldable
CW106C (2.1293) CuCrZr C18150 CC102
Products
Strips / foils
Sheets / plates
Profiles
Bars
Density: 8,91
Composition
Cu
≤ 0,2 %
Cr
≤ 0,65 %
Zr
min. 0,05 % / max. 0,8 %
Scopes
plastics engineering
mold construction
resistance welding, especially continuous welding with strong point sequence
heavy current engineering electrode arm
heat dissipation in tools
on-/offshore applications
control and instrument elements
membranes
contacts, plugs, plug connections
Features
electrode material
very high rigidity
medium electric conductivity
high thermal conductivity
CW111C (2.0855) CuNi2Si C64700
Products
Strips / foils
Pipes
Bars
Density: 8,8
Composition
Cu
Rest
Fe
≤ 0,20 %
Mn
≤ 0,10 %
Ni
min. 1,6 % / max. 2,5 %
Pb
≤ 0,20 %
Si
min. 0,4 / max. 0,8 %
Sonstige
≤ 0,30 %
Scopes
engineering
electrical engineering
high-strength bolts
plain bearing technology
chemical apparatus engineering
die-forged parts
catenary clamps
Features
curable
excellent hot and cold forming properties
very good corrosion resistance
high rigidity and resistance possible through tempering
good anti-friction properties, wear resistance
good electrical conductivity
CW118C (2.1546) Cu-TeP C14500
Products
Sheets / plates
Bars
Density: 8,94
Composition
Cu+Ag
> 99,3 %
P
min. 0,004 % / max. 0,012 %
Te
min. 0,4 % / max. 0,7 %
Scopes
welding machine nozzles
fasteners
as conductors in white goods (e.g. washing machines) and for instance in coffee machines
Features
suitable for MIG, TIG, WIG and laser welding
very good hot and cold forming properties
very good punching and deep drawing properties
excellent machinability
suitable for hard and soft soldering
CW307G (2.0966) CuAl10Ni C95500 U-A10N
Products
Pipes
Round blanks / rings
Forgings
Bars
Cuts (waterjet, plasma, shear, laser-cut or sawn)
Density: 7,6
Composition
Al
min. 8,5 % / max. 11,0 %
Ni
min. 4,0 % / max. 6,5 %
Fe
min. 3,5 % / max. 5,5 %
Mn
≤ 3,0 %
Cu
Rest
Scopes
plates for capacitor and heat transfer floors
shafts, screws and wear parts
control units for hydraulics
superheated steam fittings
mechanically and chemically stressed parts in engineering, shipbuilding and mining
Features
high strength even at higher temperatures
high fatigue strength
resistant against neutral, acidic and watery media as well as seawater
good resistance against scaling, erosion and cavitation
very high resistance
good anti-friction properties
CW502L (2.0240) CuZn15 C2300 2873
Products
Strips / foils
Pipes
Density: 8,8
Composition
Cu
≤ 85 %
Zn
Rest
Scopes
jewellery and metal goods
electrical engineering components
building façade
Features
highly malleable
corrosion resistant against fresh water, neutral or alkaline saline solutions, organic compounds, and land, sea and industrial atmospheres
not resistant against acid, moist sulphur compounds, moist ammonia in stressed condition
minor sensitivity to stress corrosion
good cold forming properties
very well suited for galvanizing, dip soldering and soft soldering
CW702R (2.0460) CuZn20Al2
Products
Strips / foils
Sheets / plates
Pipes
Bars
Density: 8,3
Composition
Cu
min. 76,0 % / max. 79,0 %
Zn
Rest
Al
min. 1,8 % / max. 2,3 %
As
min. 0,020 % / max. 0,035 %
Scopes
desalination plant
capacitors and heat exchangers
Features
high corrosion and erosion resistance in seawater
resistant to dezincification
insensitive to stress corrosion in unstressed condition
CW713R (2.0550) CuZn40Al2
Products
Pipes
Forgings
Bars
Composition
Cu
min. 57 % / max. 59 %
Mn
min. 1,5 % / max. 3 %
Si
min. 0,3 / max. 1,3 %
Al
min. 1,3 % / max. 2,3 %
Zn
Rest
Ni
≤ 1,00 %
Fe
≤ 1,00 %
Sn
≤ 0,40 %
Pb
min. 0,2 / max. 0,8 %
Sonstige
≤ 0,30 %
Scopes
engineering
automotive engineering
plain bearing elements
hot-forged parts
pins, blanks, rounds
condenser and oil cooling pipes
Features
average machinability
good aptitude for mechanical polishing
good resistance to fresh and seawater, neutral or alkaline solutions, organic compounds as well as land, sea and industrial atmospheres
increased scale resistance
not resistant to acids and sulphur compounds
EN 10152
Products
Sheets / plates
Strips / foils
Bulb plates and cuts
Composition
Scopes
Features
EN 10152, Electrolytically zinc coated cold rolled steel flat products for cold forming - Technical delivery conditions

We supply the following types of steel:

Steels for cold forming:

  • DC01+ZE: Drawing quality (material number 1.0330)
  • DC03+ZE: Drawing quality (material number 1.0347)
  • DC04+ZE: Special deep drawing quality (material number 1.0338)
  • DC05+ZE: Special deep drawing quality (material number 1.0312)

with chemical composition and mechanical properties in accordance with the requirements of EN10152.

The available coating masses, designs and surface types

  • Coating mass: ZE25/25, ZE50/50, ZE75/75, ZE100/10

Surface type: surface A, surface B

Surface treatment (surface protection)

  • P phosphated
  • PC phosphated and chemically treated
  • C chemically passivated
  • PCO phosphated, chemically treated and oiled
  • CO chemically passivated and oiled
  • PO phosphated and oiled
  • O oiled
  • S sealed
  • U without surface treatment

Available dimensions:

  • Thickness: 0.40 to 4.0 mm
  • Width: 900-1500 mm with tolerances according to EN10143 or by special agreement
  • Slit strip from 10 mm
  • Sheets 1000 - 1500 x 2000 - 6000 mm.

Coil or package weights: 1 - 10 mt by agreement

EN 10169
Products
Sheets / plates
Strips / foils
Bulb plates and cuts
Composition
Scopes
Features
EN10169, Continuously organic coated (coil coated) steel flat products - Part 1 - 3:

We supply the following types of steel:

Soft steels for cold forming:

  • DX51D: Machine folded grade (material number 1.0226)
  • DX52D: Drawing quality (material number 1.0350)
  • DX53D: Deep drawing quality (material number 1.0355)

Steels for use in the building industry:

  • S220GD (material number 1.0241)
  • S250GD (material number 1.0242)
  • S280GD (material number 1.0244)
  • S320GD (material number 1.0250)
  • S350GD (material number 1.0529)

with chemical composition and mechanical properties in accordance with the requirements of EN10346.

The available coating masses:

  • Sheet metal with zinc coating

    • Coating mass: Z100, Z140, Z200, Z225, Z275.

  • Sheet metal with zinc-aluminium coating:

    • Coating mass: ZA095, ZA130, ZA185, ZA200, ZA255ZF100, ZF120

  • Sheet metal with aluminium-zinc coating:

    • Coating mass: AZ100, AZ150, AZ185

  • Electrolytically zinc coated sheet steel:

    • Coating mass: ZE25/25, ZE50/50, ZE75/75, ZE100/100

Organic coatings and conventional layer thickness ranges in microns:

Liquid finishes

  • Acrylate AY (5 to 25)
  • Epoxy EP (3 to 20)
  • Polyester SP (5 to 30)
  • Polyamide-modified polyester SP-PA (15 to 50)
  • High durability polyester HDP (25 to 60)
  • Polyamide-modified high durability polyester HDP-PA (15 to 50)
  • Polyurethane PUR (10 to 60)
  • Polyamide modified polyurethane PUR-PA (10 to 50)
  • Polyvinylidene fluoride PFDV (20 to 60)
  • Polyvinyl chloride plastisol PVC (P) (40 to 200)

Powder finishes

  • Polyester SP (PO) (30 to 100)

Foils

  • Polyvinyl chloride PVC (F) (50 to 800)
  • Polyvinyl fluoride PVF (F) (38)
  • Polyethylene PE (F) (50 to 300)
  • Polyethylene terephthalate PET (F) (15 to 150)
  • Polypropylene PP (F) (30 to 200)

Available dimensions:

  • Thickness: 0.15 - 3.0 mm
  • Width: 900-1500 mm with tolerances according to EN10143 or by special agreement
  • Slit strip from 10 mm
  • Sheets 1000 - 1500 x 2000 - 6000 x mm.

Coil or package weights: 1 - 10 mt by agreement.

The coil coated steel sheets we deliver meet the strictest requirements of our customers and are factory-tested in accordance with the provisions of

  • EN 13523, Coil coated metals - Test methods - Part 0 to 23.

EN 10346
Products
Sheets / plates
Strips / foils
Bulb plates and cuts
Composition
Scopes
Features
EN 10346, Continuously hot-dip coated steel strip and sheet products - Technical delivery conditions:

We supply the following types of steel:

Soft steels for cold forming:

  • DX51D: Machine folded grade (material number 1.0226)
  • DX52D: Drawing quality (material number 1.0350)
  • DX53D: Deep drawing quality (material number 1.0355)
  • DX54D: Special deep drawing quality (material number 1.0306)

Steels for use in the building industry:

  • S220GD (material number 1.0241)
  • S250GD (material number 1.0242)
  • S280GD (material number 1.0244)
  • S320GD (material number 1.0250)
  • S350GD (material number 1.0529)
  • S550GD (material number 1.0531)

with chemical composition and mechanical properties in accordance with the requirements of EN10346.

The available coating masses, designs and surface types:

  • Sheet metal with zinc coating

    • Coating mass: Z100, Z140, Z200, Z225, Z275.
    • Versions: Conventional Flower (N), small flower (M)
    • Surface type: Conventional surface (A), improved surface (B), best surface (C)

  • Sheet metal with zinc-iron coating:

    • Coating mass: ZF100, ZF120
    • Versions: Conventional flower (N)
    • Surface type: Conventional surface (A), improved surface (B), best surface (C)

  • Sheet metal with zinc-aluminium coating:

    • Coating mass: ZA095, ZA130, ZA185, ZA200, ZA255ZF100, ZF120
    • Versions: Conventional flower (N)
    • Surface type: Conventional surface (A), improved surface (B), best surface (C)

  • Sheet metal with aluminium-zinc coating:

    • Coating mass: AZ100, AZ150, AZ185
    • Versions: Conventional flower (N)
    • Surface type: Conventional surface (A), improved surface (B), best surface (C)

  • Sheet metal with aluminium-silicon coating:
  • Coating mass: AS060, AS080
  • Versions: Conventional flower (N)
  • Surface type: Conventional surface (A), improved surface (B), best surface (C)

Surface treatment (surface protection):

  • chemically passivated: C;
  • oiled: O;
  • chemically passivated and oiled: CO;
  • phosphated: P;
  • phosphated and oiled: PO;
  • sealed: S.

Available dimensions:

  • Thickness: 0.15 - 5.0 mm
  • Width: 900-1500 mm with tolerances according to EN10143 or by special agreement
  • Slit strip from 10 mm
  • Sheets 1000 - 1500 x 2000 - 6000 mm.

Coil or package weights: 1 - 10 mt by agreement.

Titanium Grade 01 (3.7025) 3.7025 R50250
Products
Strips / foils
Sheets / plates
Profiles
Pipes
Pipe fittings
Round blanks / rings
Forgings
Bars
Drawing profiles
Cuts (waterjet, plasma, shear, laser-cut or sawn)
Density: 4,51
Composition
C
≤ 0,1 %
Fe
≤ 0,2 %
H
≤ 0,015 %
N
≤ 0,03 %
O
≤ 0,18 %
Ti
≤ 99,5 %
Scopes
medical technology
eyeglass frames
Features
grade 1 offers the highest corrosion resistance and formability, but the lowest resilience
Titanium Grade 02 (3.7035) 3.7035 R50400
Products
Strips / foils
Sheets / plates
Profiles
Pipes
Pipe fittings
Round blanks / rings
Forgings
Bars
Drawing profiles
Cuts (waterjet, plasma, shear, laser-cut or sawn)
Density: 4,51
Composition
C
≤ 0,1 %
Fe
≤ 0,3 %
H
≤ 0,015 %
N
≤ 0,03 %
O
≤ 0,25 %
Ti
≤ 99,2 %
Scopes
medical technology
capacitors and coolers in power plants
heat exchangers and pipe systems for seawater and brackish water
jewellery industry
zinc coating baths and galvanizing technology
cooling and air conditioning technology
components for flue gas desulfurization systems
aerospace technology
Features
advantageous ratio of strength and density
good ductility and workability
good creep strength
good corrosion resistance in oxidizing media
Titanium Grade 03 (3.7055) 3.7055 R50550
Products
Strips / foils
Sheets / plates
Profiles
Pipes
Pipe fittings
Round blanks / rings
Forgings
Bars
Drawing profiles
Cuts (waterjet, plasma, shear, laser-cut or sawn)
Density: 4,51
Composition
C
≤ 0,1 %
Fe
≤ 0,3 %
H
≤ 0,015 %
N
≤ 0,05 %
O
≤ 0,35 %
Ti
≤ 99,1 %
Scopes
medical technology
capacitors and coolers in power plants
heat exchangers and pipe systems for seawater and brackish water
jewellery industry
zinc coating baths and galvanizing technology
cooling and air conditioning technology
components for flue gas desulfurization systems
aerospace technology
Features
advantageous ratio of strength and density
good ductility and workability
good creep strength
good corrosion resistance in oxidizing media
3.7065 R50700
Products
Strips / foils
Sheets / plates
Profiles
Pipes
Pipe fittings
Round blanks / rings
Forgings
Bars
Drawing profiles
Cuts (waterjet, plasma, shear, laser-cut or sawn)
Density: 4,51
Composition
C
≤ 0,1 %
Fe
≤ 0,5 %
H
≤ 0,015 %
N
≤ 0,05 %
O
≤ 0,4 %
Ti
≤ 99 %
Scopes
medical technology
capacitors and coolers in power plants
heat exchangers and pipe systems for seawater and brackish water
jewellery industry
zinc coating baths and galvanizing technology
cooling and air conditioning technology
components for flue gas desulfurization systems
aerospace technology
Features
advantageous ratio of strength and density
good ductility and workability
good creep strength
good corrosion resistance in oxidizing media
Titanium Grade 05 (3.7164) 3.7164 R56400
Products
Strips / foils
Sheets / plates
Profiles
Pipes
Pipe fittings
Round blanks / rings
Forgings
Drawing profiles
Cuts (waterjet, plasma, shear, laser-cut or sawn)
Density: 4,43
Composition
Al
≤ 6,0 %
Fe
≤ 0,25 %
V
≤ 4,0 %
O
≤ 0,2 %
Ti
≤ 90 %
Scopes
components for aerospace technology
components and sonotrodes for ultrasonics
components in engine technology
sport accessories (bicycles, boat accessories, etc.)
Features
curable
excellent corrosion properties due to superb oxide coating
maximum application temp. 400°C
Titanium Grade 07 (3.7235) 3.7235 R52400
Products
Strips / foils
Sheets / plates
Profiles
Pipes
Pipe fittings
Round blanks / rings
Forgings
Bars
Drawing profiles
Cuts (waterjet, plasma, shear, laser-cut or sawn)
Composition
C
≤ 0,08 %
Pd
min. 0,12 % / max. 0,25 %
H
≤ 0,02 %
N
≤ 0,03 %
Ti
Rest
Fe
≤ 0,30 %
O
≤ 0,25 %
Scopes
chemical industry, especially with highly aggressive and chloride-containing media
Features
better corrosion resistance to reducing solutions than pure titanium
lower risk of crevice corrosion than with commercially pure titanium especially in chloride-containing media
Titanium Grade 11 (3.7225) 3.7225 R52550
Products
Strips / foils
Sheets / plates
Profiles
Pipes
Pipe fittings
Round blanks / rings
Forgings
Bars
Drawing profiles
Cuts (waterjet, plasma, shear, laser-cut or sawn)
Composition
C
≤ 0,08 %
Pd
min. 0,12 % / max. 0,25 %
H
≤ 0,02 %
N
≤ 0,03 %
Ti
Rest
Fe
≤ 0,20 %
O
≤ 0,18 %
Scopes
chemical industry, especially with highly aggressive and chloride-containing media
Features
better corrosion resistance to reducing solutions than pure titanium
lower risk of crevice corrosion than with commercially pure titanium especially in chloride-containing media
Titanium Grade 12 (3.7105) 3.7105 R53400
Products
Strips / foils
Sheets / plates
Profiles
Pipes
Pipe fittings
Round blanks / rings
Forgings
Bars
Drawing profiles
Cuts (waterjet, plasma, shear, laser-cut or sawn)
Composition
C
≤ 0,08 %
Mo
min. 0,20 % / max. 0,40 %
Ni
min. 0,60 % / max. 0,90 %
N
≤ 0,03 %
Ti
Rest
Fe
≤ 0,30 %
O
≤ 0,25 %
H
≤ 0,02 %
Scopes
chemical industry
pressure container construction
Features
better corrosion resistance to reducing solutions than pure titanium
lower risk of crevice corrosion than with commercially pure titanium especially in chloride-containing media

All information is supplied without liability reg. e.g. mistakes, completeness or topicality.